epoxy-floor-coating-comparison--colored-sand-self-leveling-8-colours-ce/isoepoxy-colored-sand-self-leveling-floor-coating--standard-grade-25kg-8-colours, epoxy-floor-coating-comparison--colored-sand-self-leveling-8-colours-ce/isoepoxy-colored-sand-self-leveling-floor-coating--standard-grade-25kg-8-colours, /epoxy-colored-sand-floor-coating
Inquisitio
epoxy-floor-coating-comparison--colored-sand-self-leveling-8-colours-ce/isoepoxy-colored-sand-self-leveling-floor-coating--standard-grade-25kg-8-colours, epoxy-floor-coating-comparison--colored-sand-self-leveling-8-colours-ce/isoepoxy-colored-sand-self-leveling-floor-coating--standard-grade-25kg-8-colours, 
Inquisitio

Epoxy Colored Sand Self-Leveling Floor Coating – Standard Grade, 25kg, 8 Colours

Standardis coloratus sabinus epoxy self-leveling pavimentum, 25 kg bucket. Granitiformis punctatus finis in octo coloribus standardibus (HC51-011 ad 018). Resistentia ad chemicas, resistentia ad abrasionem, continuus pavimentum pro fabricis, magazinis et stationibus automobilium. MOQ 1 tonna. Certificatum CE.

Pete Citationem
  • Conspectus

Conspectus

Comparatio Revestimenti Soli Epoxy: Seligens Systema Rectum pro Usu Industriali

Comparatio accurata revestimenti soli epoxy aestimat robur compressionis, resistentiam ad chemicas, spissitudinem pelliculae siccae, requisita installationis, statum certificationis, et pretium totale per totam vitam — non solum pretium unitatis. Haec descriptio structurata comparat Revestimentum Solum Epoxy Sabuli Colorati Auto-Nivelans (Gradus Normalis) ad alternativas normales secundum dimensiones quae determinant praestantiam longae durationis in ambientes magazinorum, fabricarum, et logisticae.

Product Overview

Sistēma no divām komponentēm — epoksīds, kas sajaucis ar krāsotu kvartsa smiltīm. Šī sistēma sastāv no epoksīda gruntējuma, pamata pārklājuma ar iemaisītām kvartsa smiltīm un pašnivelojoša augšējā pārklājuma, kas izlīdzinās līdz gludam, vienmērīgam virsmas slānim ar minimālu grīdas līmeņošanas darbu. Šī pašnivelojošā īpašība samazina prasības pret uzstādītāju kvalifikāciju un nodrošina vienmērīgu virsmas kvalitāti lielos grīdu apgabalos bez speciālas iekārtas — praktisks priekšrocības rūpnieciskiem grīdu projektiem ar lielu apjomu.

epoxy-colored-sand-floor-coating-1.png

Epoksīda grīdu pārklājumu salīdzinājums: Veiktspējas dimensijas

salīdzinājums ar standarta epoksīda krāsu — izturība un dzīves cikla izmaksas

Pictura epoxida monocapsularis standardis spissitudinem pelliculae siccae 0.1–0.3 mm praebet, quae ad loca levis usus apta est. Hoc systema se ipsum aequans spissitudinem pelliculae siccae 1.5–3.0 mm et robur compressivum ≥ 70 MPa praebet — differentia performance clara sub trafico industriali continuo. Ex perspectiva reditus investitionis in pavimentis magazinorum, pictura standardis in locis intensi usus saepe post biennium ad triennium renovanda est; systema se ipsum aequans longiorem vitam functionalem habet, quod praemium sui pretii per periodum aestimationis quinque ad septem annorum solvit per minorem frequentiam renovandi et minorem tempus in quo facillitas non operatur.

Coating arenae quartziferae resistentis ad chemicas vs. systemata pellicularum tenuium

Ubi pavimenta cotidie oleis, siccantibus, acidis dilutis aut alcalibus exponuntur, stratum sabuli quartzici resistentis contra chemicas substantias protectionem praebet, quam tenuia strata alternativa non praestare possunt. Maturata matrice epoxy bicomponente cum aggregato quartzico inclusa penetrationem chemicam resistit, dum integritas superficiei sub gravi trafico servatur. Compositio chymica tam magni momenti est quam spissitudo strati — hoc systema speciatim ad loca industrialia ubi chymicae substantiae adsunt fabricatum est.

Specificationes Technicae

Parametrum Valor
Typus Epoxy bicomponente + sabulum quartzicum coloratum
Metam Autonivelans graniticum punctatum
Colores normales 8 colores (HC51-011 usque ad HC51-018)
Spissitudo Pelliculae Siccae 1,5–3,0 mm
Fortitudo compressiva ≥ 70 MPa
Robustitas Tractionis ≥ 1,5 MPa
Resistentia ad abrasionem ≤ 0,03 g (Taber CS-17, 1000 cycli)
Chemical Resistentia Olea, siccantia, acida diluta et alcalia
Ratio applicationis 3,0–5,0 kg/m²
Emballatio 25 kg/secius
MOQ 1 Ton
Certificationes CE, ISO 14001

CE marking confirms European construction product compliance. ISO 14001 certification confirms the facility meets internationally recognised environmental management standards — required for projects with sustainability procurement policies or regulated-market import conditions.

Applicationem Environments

Warehouses and Logistics Centres

≥ 70 MPa compressive strength and ≤ 0.03 g abrasion resistance (Taber CS-17, 1000 cycles) withstand forklift traffic, pallet loads, and industrial cleaning. The warehouse floor ROI case rests on extended service intervals versus painted or untreated concrete floors.

Factory and Industrial Plant Floors

The chemical resistant quartz sand coating — resisting oils, fuels, dilute acids, and alkalis — reduces contamination risk in manufacturing environments. Available in 8 standard colours (HC51-011 to HC51-018) for production zone colour-coding in ISO-certified facilities.

Car Parks and Showrooms

Finis granit-speckle convenit ad parkingia automobilium supra et sub gradum, ad aedificia ostentationis, et ad spatia mercatoria. Colorum RAL/Pantone ad mensuram disponibilis praeter octo colores normales in deposito.

epoxy-colored-sand-floor-coating-scene.png


Installatio pavimenti industrialis auto-nivelantis

Installatio correcta pavimenti industrialis auto-nivelantis determinat performance superficiei longi temporis. Processus quinque graduum:

  • Praeparatio Substrati: Tere aut pulvere concretum ad CSP 3–4. Repara rimas et vacua. Praeparatio inadecvata est causa prima defectus adhaesionis.
  • Applicatio Primae Cocturae: Applica primarium epoxy; cura 4–8 horas ad 20°C ut substratum obsignes et integritatem adhaesionis constituas.
  • Coat basis cum sabulo arenaceo: Applica coat basis epoxy per rulotum; sparge sabulum quartzum coloratum dum humectum est ut textura et crassitudo augeantur.
  • Coat superior auto-nivelans: Misce duos componentes ad rationem specificatam; diffunde per squeegee dentatum et revolve per rulotum spinosum ut aer inclusus emittatur.
  • Coagulatio: 24 horas antequam transitus pedum permittitur; 7 dies antequam transitus vehiculorum ad 20°C.


Cur nos eligere?

  • 20 annos de fabricatio de recubrimentos epoxy pro pavimenta, con qualitate constante de formulatio bicomponente
  • Certificatus ISO 9001 et ISO 14001; capacitas productoria annua 11 000 tonnae
  • 8 colores standard in stock; possibilitas de adaptatio ad colores RAL/Pantone ad petitionem
  • Quantitas minima ordinabilis: 1 tonna per color; productio sub marca propria (OEM) vel sub etiquetta privata, cum imballatio personalis de 25 kg
  • Documentation complete: certificato CE, COA, TDS, MSDS
  • Supporto technico pro evaluatione substrati et calculo rationis applicationis

details (1).png

De Societate

Shandong Dingtai Waterproof Technology Co., Ltd. est fabricator praecipuus in Taitou Industrial Park, maximo centro productionis materialium impermeabilium Sinarum. Ut societas iuribus propriis ad importandum et exportandum, producta nostra iam vendita sunt in regionibus et nationibus per totum orbem, ut in America Septentrionali, Asiae Sudorientalis, Americae Meridionalis, Africae, Europa et Medio Oriente. Fidelitas nostra ad qualitatem praestantem et ad servitium fidelem nobis famam internationalem validam et praesentiam mercatoriam crescentem meruit.

details (2).png

details (3).png

Quaestiones Frequenter Rogatae

Q1: Cur nos eligere debes?

A: Nos sumus fabricatores periti, et optima producta, pretia competitiva et servitium egregium praebere possumus.

Q2: Num exemplaria praebetis? Gratisne sunt an extra?

A: Ita, exemplaria gratis pro inspectione qualitatis praebere possumus. Secundum regulas nostrae societatis, tu onera vehiculi sustinere debes; sed onera vehiculi tibi restituemus si ordinem facis.

Q3: Quae est tempus expeditionis?

A: VII–XV dies post acceptum depositum vel litteras creditoris ad visum.

Q4: Quomodo tua fabrica de qualitate controlat?

A: Qualitas est prioritas. Semper magnopere curamus de controllo qualitatis ab initio usque ad finem. Habemus professionalem turmam QA/QC ut qualitatem garantiamus.

Q5: An ordines OEM vel ODM accipitis?

A: Ita, tam OEM quam ODM accipimus pro clientibus.

Q6: Quae sunt vestrae condicionis de delatione?

A: EXW, FOB, ClF, et cetera accipere possumus. Unam eligere potes quae tibi maxime conveniat.

Q7: Quae est ratio solvendi?

A: TT, L/C ad visum, West Union, Online Bank Payment.

Q8: Estisne societas mercatoria an fabricator?

A: Fabricatores sumus. Ideo pretium inferius habemus quam societates mercatoriae.

Epoxy Colored Sand Self-Leveling Floor Coating – Standard Grade, 25kg, 8 Colours

Standardis coloratus sabinus epoxy self-leveling pavimentum, 25 kg bucket. Granitiformis punctatus finis in octo coloribus standardibus (HC51-011 ad 018). Resistentia ad chemicas, resistentia ad abrasionem, continuus pavimentum pro fabricis, magazinis et stationibus automobilium. MOQ 1 tonna. Certificatum CE.

Pete Citationem

Fortasse etiam tibi placebit

Accipe Aestimationem Gratuitam

Legatus noster te mox contactabit.
Epistula electronica
Mobilis/Whatsapp
Nomen
Nomen societatis
Nuntius
0/1000