bitumen-waterproof-tape--15mm-aluminum-foil-surface-roof-seam--metal-flashing, bitumen-waterproof-tape--15mm-aluminum-foil-surface-roof-seam--metal-flashing, /bitumen-waterproof-tape
Bitumen waterproof tape with aluminium foil surface, 1.5 mm thick. UV-resistant, heat-reflective sealing for roof seams, metal roof laps, HVAC duct joints, and exposed flashing. Width 100–600 mm, length 7.5–20 m, custom. CE certified.
This 1.5mm bitumen waterproof tape combines an SBS modified bitumen adhesive compound with a bright aluminum foil top surface, delivering UV resistance, vapour barrier performance, and reliable adhesion to metal substrates in a single self-adhesive format. It seals exposed roof membrane laps, metal roofing panel joints, parapet cap flashing, and HVAC duct seams where long-term outdoor adhesion is required without a protective overlay. CE and ISO 14001 certified, this bitumen waterproof tape is available in widths from 100mm to 600mm with custom roll lengths from 7.5m to 20m. 
Superficies folii aluminium reflectit radiationem solarem, impedens disruptionem oxydativam bituminis SBS causatam ab UV. Pro lineis iuncturarum perpetuo expositis – ut laminae crista, capsulae parapetorum, aut superpositionibus tectorum cum costis erectis – haec fascia bituminosa impermeabilis prolongat vitam functionalem adhaesivi comparata ad alternativas cum superficie PE, quae bitumen in marginibus pelliculae partim exponunt, ubi degradatio ab UV primum incipit.
Modificatio SBS dat composito bituminoso recuperationem elastomeriam sub cyclis expansionis thermalis. Adhaesio per avulsionem attingit ≥1.5 N/mm et fortitudo tensilis ≥400 N/50mm. Haec fascia bituminosa modificata SBS adhaeret ad laminas tectorum metallicas ex ferro, aluminium, zincum-coatam, et praepinctas sine praeparatione speciali in superficiebus siccis et mundis. Experientia in campo confirmat quod defectus adhaesionis in lineis iuncturarum oriuntur ex insufficienti praeparatione superficiei, non ex ipso composito.
Stratum folii aluminium fungit ut barriera contra vaporem in iuncturis superpositis hermeticis, impedens diffusionem vaporis aquosi per rimas membranarum tecti isolatarum. Haec fascia adhaesiva pro tectis ex folio aluminium non solum hermetice obsignat, sed etiam impedit penetrationem vaporis in una applicatione, minuens periculum condensationis et deterioris isolationis in structuris climatum frigidorum et humiditatis altioris.
Superficies reflectens folii in hac fascia pro tegendo, quae resista radiationi ultraviolettae, minuit differentiam temperaturarum in interfacie adhaesivi durante maxima incursione solari, diminuens fatigationem propter cyclum thermicum in iuncturis patentibus. Tabulae tectorum ex aluminium et zinc habent maiores coefficientes dilationis thermalis quam tabulae ex ferro, ideoque reductio stress thermici in iuncturis metallorum dissimilium praesertim necessaria est in installationibus climatum tropicalium et aridorum.
| Parametrum | Valor |
|---|---|
| Modifier | SBS Modified Bitumen |
| Superficies Superior | Folium aluminium lucidum |
| Liner liberatorius | Pellicula silicea |
| Crassitudo | 1.5mm |
| Intervallum Largitatis | 100–600 mm (ad libitum) |
| Roll Longitudo | 7,5–20 m (ad libitum) |
| Adhaerentia Detrahenda | ≥1,5 N/mm |
| Robur Tensile | ≥400 N/50 mm |
| Flexibilitas ad Temperaturam Infra | -20°C |
| Impermeabilitas Aquae | Successus ad 0,3 MPa |
| Certificationes | CE, ISO 14001 |
In condicionibus tecti apertis, fascia bituminosa impermeabilis subicit expositionem continuam ad UV, cyclum thermicum, et abrasionem pluviam simul. Superficies folii aluminium directe sustinet onus UV; compositum SBS manet flexibile per cyclum temperaturarum a temperata ad tropicam. Latitudo 100–600 mm amplectitur latitudines standard lap et necessitates latiores pontificationis iuncturarum. Fugae in campo ad iuncturas tectorum congregantur ad margines superpositionis et ad puncta terminationis, non trans faciem planam – qualitas adhaesionis marginis tempore applicationis est variabilis maxime critica.
Hoc fasciculum adhaesivum pro tectis ex folio alluminii adhaeret ad substrata ferro-ferrea, ferro-alluminia, et metalla picta ad metalla picta sine praeprimario. Pro detaliis in culmine et in lamina parapetali, usus huius fasciculi adhaesivi pro iuncturis tectorum vitat tempus indurationis sigillantium liquidorum, dum spissitudo adhaesivi constans praebetur. Superficies folii creavit finitionem metallicam visibiliter constantem, aptam pro confectionibus tectorum metallicis expositis.
Iuncturae isolamenti ducuum et tuborum HVAC involvunt substrata mixta – ducos metallicos, insulatum rigidum ex spuma, tabulas ex fibra vitrea. Compositum bituminosum autoadhaesivum se accommodat his superficiebus in iuncturis transitionis materialium absque apparatu calefaciente. Hoc fasciculum bituminosum impermeabile statim adhaeret ut sit hermeticum in applicatione, idoneum ergo tam pro manutenentia ordinata quam pro reparationibus urgentibus.


Shandong Dingtai Waterproof Technology Co., Ltd. est fabricator praecipuus in Taitou Industrial Park, maximo centro productionis materialium impermeabilium Sinarum. Ut societas iuribus propriis ad importandum et exportandum, producta nostra iam vendita sunt in regionibus et nationibus per totum orbem, ut in America Septentrionali, Asiae Sudorientalis, Americae Meridionalis, Africae, Europa et Medio Oriente. Fidelitas nostra ad qualitatem praestantem et ad servitium fidelem nobis famam internationalem validam et praesentiam mercatoriam crescentem meruit. 

Q1: Cur nos eligere debes?
A: Nos sumus fabricatores periti, et optima producta, pretia competitiva et servitium egregium praebere possumus.
Q2: Num exemplaria praebetis? Gratisne sunt an extra?
A: Ita, exemplaria gratis pro inspectione qualitatis praebere possumus. Secundum regulas nostrae societatis, tu onera vehiculi sustinere debes; sed onera vehiculi tibi restituemus si ordinem facis.
Q3: Quae est tempus expeditionis?
A: VII–XV dies post acceptum depositum vel litteras creditoris ad visum.
Q4: Quomodo tua fabrica de qualitate controlat?
A: Qualitas est prioritas. Semper magnopere curamus de controllo qualitatis ab initio usque ad finem. Habemus professionalem turmam QA/QC ut qualitatem garantiamus.
Q5: An ordines OEM vel ODM accipitis?
A: Ita, tam OEM quam ODM accipimus pro clientibus.
Q6: Quae sunt vestrae condicionis de delatione?
A: EXW, FOB, ClF, et cetera accipere possumus. Unam eligere potes quae tibi maxime conveniat.
Q7: Quae est ratio solvendi?
A: TT, L/C ad visum, West Union, Online Bank Payment.
Q8: Estisne societas mercatoria an fabricator?
A: Fabricatores sumus. Ideo pretium inferius habemus quam societates mercatoriae.
Bitumen waterproof tape with aluminium foil surface, 1.5 mm thick. UV-resistant, heat-reflective sealing for roof seams, metal roof laps, HVAC duct joints, and exposed flashing. Width 100–600 mm, length 7.5–20 m, custom. CE certified.